Melting and pumping heat-resistant stainless steel fiber: The raw material is stainless steel ingot. Use an electric furnace to melt the steel ingot into a steel liquid at a temperature of 1500°C~1600°C. Then, on the surface of the molten steel, a high-speed rotating melting puller is used to approach the molten steel. The melting puller is in accordance with According to the requirements of the required steel fiber size, many grooves are carved. When the molten puller drops to the molten steel surface, the molten steel is scraped out of the groove, thrown out by the centrifugal force of high-speed rotation, and cooled into rows at a rapid speed. Water must flow through the melt puller to maintain the cooling rate. This method can produce steel fibers of different materials and sizes according to customer requirements.
For more information, please visit our website.
Advantage of refractory steel fiber
.Improve refractories performance
.Improve refractories longevity
.Improve refractories durability
.reduce furnace downtime and maintainace cost
.Size(MM):thick*diameter* length:0.3×1×25/35
.Melting point range:1425~1450(310#)
.Modulus of elasticity at 870°C:12.55Gpa
.Heat conduction at 500°C:18.7
well contains other products and information you need, so please check it out.
.Thermal expansion coefficient at 870°C:18.58
.Tensile strength at 870°C: 155MpaChemical composition
.high temperature resistance
.high tensile strength
.durable
.anti-oxidation
.damp-proof
.resistant to corrosion
.Improve refractories performance
.Improve refractories longevity
.Improve refractories durability
.reduce furnace downtime and maintainace cost
the raw material is stainless steel ingots, using electric stoves which melt the stainless steel ingots to become 1500 ~ 1600 ℃ steel liquid,and then with a grooved high speed rotating melt-extracting steel wheel which produces wires that meets are our customers’ specific requirements. When melting down to a wheel steel liquid surface, the liquid steel blow out by slot with centrifugal force at extremely high speed with cooling forming. Melting wheels with water keep the cooling speed. This method is done to produce different material, different sizes of steel fibers.specification1.Q: What is the minimum order amount?A: Orders from one metric ton are possible.2.Q: What’s the delivery time?A: 7~15 days after T/T prepayment or L/C date.3.Q: Can I get some samples free?A: Free sample can be provided if you require to check the quality.4.Q: How can we trust you?A: Harvest has been cooperated with ALIBABA on trade assurance since.5.Q: If you don't know your project need what type of steel fiber,what should you do?A: Please feel free to contact us and tell us the details about you project, for example purposes, aggregate size and compressive strength,etc. We can design and manufacture for you.
Melting and pumping heat-resistant stainless steel fiber: The raw material is stainless steel ingot. Use an electric furnace to melt the steel ingot into a steel liquid at a temperature of 1500°C~1600°C. Then, on the surface of the molten steel, a high-speed rotating melting puller is used to approach the molten steel. The melting puller is in accordance with According to the requirements of the required steel fiber size, many grooves are carved. When the molten puller drops to the molten steel surface, the molten steel is scraped out of the groove, thrown out by the centrifugal force of high-speed rotation, and cooled into rows at a rapid speed. Water must flow through the melt puller to maintain the cooling rate. This method can produce steel fibers of different materials and sizes according to customer requirements.
Advantage of refractory steel fiber
.Improve refractories performance
.Improve refractories longevity
.Improve refractories durability
.reduce furnace downtime and maintainace cost
.Size(MM):thick*diameter* length:0.3×1×25/35
.Melting point range:1425~1450(310#)
.Modulus of elasticity at 870°C:12.55Gpa
.Heat conduction at 500°C:18.7
.Thermal expansion coefficient at 870°C:18.58
.Tensile strength at 870°C: 155MpaChemical composition
.high temperature resistance
.high tensile strength
.durable
.anti-oxidation
.damp-proof
.resistant to corrosion
.Improve refractories performance
.Improve refractories longevity
.Improve refractories durability
.reduce furnace downtime and maintainace cost
the raw material is stainless steel ingots, using electric stoves which melt the stainless steel ingots to become 1500 ~ 1600 ℃ steel liquid,and then with a grooved high speed rotating melt-extracting steel wheel which produces wires that meets are our customers’ specific requirements. When melting down to a wheel steel liquid surface, the liquid steel blow out by slot with centrifugal force at extremely high speed with cooling forming. Melting wheels with water keep the cooling speed. This method is done to produce different material, different sizes of steel fibers.specification1.Q: What is the minimum order amount?A: Orders from one metric ton are possible.2.Q: What’s the delivery time?A: 7~15 days after T/T prepayment or L/C date.3.Q: Can I get some samples free?A: Free sample can be provided if you require to check the quality.4.Q: How can we trust you?A: Harvest has been cooperated with ALIBABA on trade assurance since.5.Q: If you don't know your project need what type of steel fiber,what should you do?A: Please feel free to contact us and tell us the details about you project, for example purposes, aggregate size and compressive strength,etc. We can design and manufacture for you.